When decapusating semiconductors (computer chips), we use concentrated sulfuric, It can sit on the mold compound for quite a while with little effect at room temp. We set the parts on a hot plate to get them warmed up (too hot to touch) and then it eats away the mold compound in a few seconds.

What I am saying is, the added temp will make it potentially VERY fast, so do some testing and get a good rythem going at a controllable temperature.